MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Crucible Steel 410 Chromium Steel
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Crucible 410 is a hardenable chromium steel which is adaptable for general purpose corrosion resisting and heat resisting applications. This grade is magnetic at times.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.70 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 155
Tensile Strength, Ultimate 75000 psi
Tensile Strength, Yield 45000 psi
@Strain 0.2 %
Elongation at Break 30 %in 2"
Reduction of Area 75 %
Tensile Modulus 29000 ksi
Poissons Ratio 0.32Calculated
Shear Modulus 11000 ksi
Izod Impact Unnotched 90.0 ft-lb
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000569 ohm-cm
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.50 µin/in-°F
@Temperature 0.000 - 100 °C
 5.60 µin/in-°F
@Temperature 0.000 - 316 °C
 6.50 µin/in-°F
@Temperature 0.000 - 649 °C
Thermal Conductivity 172.8 BTU-in/hr-ft²-°F
@Temperature 93.3 °C
 198 BTU-in/hr-ft²-°F
@Temperature 538 °C
Melting Point 2700 - 2790 °F
Solidus 2700 °F
Liquidus 2790 °F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 11.5 - 13.5 %
Iron, Fe >= 84.28 %As Remainder
Manganese, Mn <= 1.0 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %
 
Descriptive Properties
Endurance Limit, ksi40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Carbide, TiC
AISI 440 Stainless Steel
Titanium, Ti
AK Steel 439 Ferritic Stainless steel
Crucible Steel 430 Chromium Steel

NCRUC041 / 16034

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.