MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Nouryon Cadox L-50a VR Methyl ethyl ketone peroxide
Categories: Other Engineering Material

Material Notes: Special purpose catalyst for curing tooling gel coats and promoted unsaturated polyester resins. Low-hydrogen peroxide & high dimer content reduces gel-coat porosity and provides improved curing of vinylester resins.

CAS number: 1338-23-4

EINECS/ELINCS No.: 215-661-2

Applications: Cadox L-50a VR is a special purpose catalyst for the room temperature cure of promoted unsaturated polyester resins. CADOX L-50a VR has a low hydrogen peroxide content which provides improved curing of vinyl ester resins. Cadox L-50a VR also has a high MEKP dimer content which may provide reduced cure times in some resin systems. Cadox L-50a VR offers all the advantages of a red MEKP, except red parts. The VR series of products includes a red indicator system that virtually disappears during cure. The red is there when you need it, but not in the finished product. Visualize hot & cold spots, schrinkage problems, mass effects, thermal effects of core materials and dead flow zones in applications like vacuum infusion.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/cc
Storage Temperature <= 30.0 °C
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 60.0 °CSelf-Accelerating Decomposition Temperature
 
Descriptive Properties
AppearanceRed liquid
Content(%)8.9Total active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY461 / 285984

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.