When used with Cilbond 12E (solvent-based primer) or Cilbond 62W (water-based primer), Cilbond 80ET will bond the elastomers listed below to a range of metal and plastic substrates during the vulcanization and post-vulcanisation processes: - Natural Rubber (NR)
- Styrene Butadine Rubber (SBR)
- Polychloroprene Rubber (CR)
- Synthetic Poyisoprene Rubber (IR)
- Nitrile Rubber (NBR and XNBR)
- Hydrogenated NBR (HNBR sulphur or peroxide cured)
- Polybutadiene (BR)
- Ethylene Propylene Copolymer (EPM)
- Ethylene Propylene Diene Terpolymer (EPDM sulphur or peroxide cured and silicone modified)
- Butyl Rubber (IIR)
- Halogenated Butyl Rubber (CIIR and BIIR)
- Epichorohydrin Rubber (ECO)
- Chlorosulphonated Polyethylene (CSM/ACSM)
- Ethylene Ethyl Acrylate (Vamac®)
- Ethylene Vinyl Acetate (EVA/EVM)
- Polyacrylate (ACM)
- Chlorinated Polyethylene (CPE)
- Millable Polyurethane ( Sulphur or peroxide cured)
Cilbond 80ET also gives excellent adhesion to RFL-treated fabrics and finds uses in high-performance timing belts, hoses and carriage belts, especially where severe environments are present such as high temperatures and fluids.Information provided by HB Chemical |