Compound 3918 is a 90 durometer black colored Buna N elastomer, it is formulated with Teflon to provide internal lubrication. All materials in this compound are FDA approved. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 6 BG 915 A14 B14 B343 EO14 EO34; 7 BG 915 B14 EA14 EF11 EF21 EO14 EO34; 4 BK 915 A14 B14 EF11 EO14 Information provided by Pressure Seals Inc. |