MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® Terra HS1851 Nylon 610, Glass Reinforced
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610); Nylon 610, Glass Reinforced

Material Notes: Glass fiber-reinforced, heat-stabilized, medium-viscosity PA 610 compound for injection molding application. VESTAMID® Terra HS1851 is a glass fiber-reinforced, heat-stabilized, medium-viscosity PA 610 compound for injection molding application. The material contains about 20% glass fibers, an ageing protective agent and processing aid for a fast and even form filling. The carbonamide groups (-CO-NH-) of the polyamides form hydrogen bridge bonds between the chains of the macromolecules, thereby substantially promoting crystallinity and increasing their strength, melting point, resistance to chemicals and even water absorption. This is characteristic of all semi-crystalline polyamides. Because of its semi-crystalline morphology VESTAMID® Terra HS1851 provides a high impact strength, excellent chemical resistance (e.g. against greases, oils, alkalis and saline solutions), a low coefficient of friction and high abrasion resistance. VESTAMID® Terra HS1851 is supplied as cylindrical granules, ready for processing, in moisture-proof bags. VESTAMID® Terra is a group of new polyamides, the monomers for which are based entirely or partly on renewable raw materials.
VESTAMID® Terra HS is the polycondensation product of 1,6-hexamethylene diamine (H) and 1,10-decanedioic acid (sebacic acid-S). Because sebacic acid is derived from castor oil, VESTAMID® Terra HS is a material that is partly based on renewable resources.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccISO 1183
Water Absorption 2.6 %Sim. to ISO 62
Linear Mold Shrinkage 0.0070 cm/cmNominal; ISO 294-4, 2577
Linear Mold Shrinkage, Flow 0.0040 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPaISO 527
Tensile Strength, Yield 138 MPaISO 527
Elongation at Break 4.3 %ISO 527
 4.5 %Nominal; ISO 527
Elongation at Yield 4.0 %ISO 527
Tensile Modulus 5900 MPaISO 527
Charpy Impact Unnotched 78.0 kJ/m²
@Temperature -30.0 °C
Complete Break; ISO 179/1eU
 86.0 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eU
Charpy Impact, Notched 8.90 kJ/m²
@Temperature -30.0 °C
Complete Break; ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 26.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 124 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 223 °CISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 204 °CISO 75-1/-2
Vicat Softening Point 219 °CMethod B: 10 N, 50 K/h; ISO 306
 221 °CMethod A: 10 N, 50 K/h; ISO 306
Glass Transition Temp, Tg 49.0 °CISO 11357-1/-2
 
Processing PropertiesOriginal ValueComments
Mold Temperature 50.0 °CTest condition for mold shrinkage
 80.0 °CTest condition for mold shrinkage

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK869 / 243076

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.