MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem RETARDER RSF
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: A non-staining and non-discoloring retarder for natural and synthetic rubber compounds. Use from 0.50 to 1.3 parts per 100 phr, depending on polymer and accelerator system used. Very effective with sulfonamide systems. Effective in thiazole systems as well as low sulfur/thiuram cures. Also useful for replasticizing of slightly scorched stocks by cold mill mixing. Replaces Retarder SAFE in many applications at a lower cost. When Retarder RSF is used in natural rubber, reversion is minimized. Does not bloom at recommended amounts and no odor occurs from the use of Retarder RSF. Does not significantly change the fully cured characteristics of the compound. State-of-cure is effected less than with most other retarders.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point 77.0 - 83.0 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.50 %
 
Descriptive Properties
AppearanceCream to Tan Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH577 / 315495

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.