MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Sealants & Adhesives Painter’s Quick Dry Siliconized Acrylic Latex Caulk
Categories: Polymer; Thermoset; Silicone

Material Notes: Painter’s Quick Dry Siliconized Acrylic Latex is an advanced grade caulk that is paint-ready in as little as 20 minutes for a quicker workflow. Painter’s Quick Dry Siliconized Acrylic Latex caulk is ideal for interior and exterior projects that require durable flexibility. This formulation offers excellent adhesion to a wide variety of building materials. Painter’s Quick Dry Siliconized Acrylic Latex caulk guns out effortlessly, tools smoothly, and cleans-up easily with soap and water. This low odor and paint-friendly caulk resists cracking with and is compatible with most latex and oil paints. When fully cured, the caulk is resistant to stain-causing mold and mildew growth, creating a durable seal that is resilient and tough for long-lasting professional results.

Features: Backed by a limited 50-year durability guarantee, 20 minute paint ready and immediate spray paint ready- for a quicker workflow, Strong adhesion and flexibility – exceeds ASTM C-834, Grade -18°C flexibility requirements, Resists cracking-for long-lasting professional results, Will not fade, suitable for water and oil based paints, Cured caulk forms a waterproof seal, Low odor and low VOC (Meets CARB VOC Limits), Easy application, Soap and water clean-up.

Applications: Painter’s Quick Dry Siliconized Acrylic Latex caulk can be used in a wide variety of interior and exterior applications, including trim, crown molding, baseboards, vents and around doors, windows.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.61 g/ccUncured
Solids Content 74 - 78 %By weight. Uncured.; ASTM C1250
Volatile Organic Compounds (VOC) Content <= 33 g/lUncured. Excluding water & exempt compounds
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50ASTM 661
Elongation at Break 500 %ASTM D412
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 158 °F
Minimum Service Temperature, Air -15.0 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 100 °CApplication Temp
Cure Time 24.0 hour3/16 inch bead size
Tack-Free Time 40.0 minASTM C679
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceSmooth & CreamyUncured.
BaseAcrylic Latex
Carb Chem Curing VOC<1.5 wt.%Uncured. Non-Chem Curing.
Clean-upDamp Disposable Cloth
ColorWhiteMAP310WT 12C
Consistency / SagPassedUncured. ASTM C693
Coverage Rate51 Lin. Ft.At 3/16" bead.
Extension Recovery and Adhesion (Glass/Al.)PassedASTM C736
Freeze/Thaw StabilityPassed / 5 Cycles at 0°FUncured. ASTM C731.
Heat Aging and Weight Lost Cracking, CaulkingPassed
Low Temperature FlexibilityPassedASTM C732
OdorSlight AcrylicUncured
Paint Ready Time20 minutes
PaintableLatex & Oil Based Paints
Peel StrengthPassedASTM C794, Dry
Stain/Color ChangePassedASTM C510
Water Ready24 hoursUncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9949 / 265761

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.