MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polyrocks Chemical 5003RM5N PP Master batch, Flame Retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Halogen-free flame retardant PP master batches based on phosphorus and nitrogen as main flame retardant elements. It improves flame retardant efficiency by synergistic effect of solidifying phase and gas-phase mechanism, and accelerating melting and dripping by catalytic mechanism to play flame retardant performance. 5003RM5N is used for adding to pp to reach UL94 V2 flammability grade, adding a certain percentage of master batches in homopolymer PP, copolymer pp ( or mixture of homopolymer pp and copolymer pp), could reach excellent flame retardant effect. It has UL certification, and meets the requirements of RoHS?SVHC?PFOS & PFOA?16P?PAHs...etc. 5003RM5N has the properties of low density, low smoke, less corrosion to moulds

Information provided by Polyrocks

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccASTM D792
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-2
@Thickness 1.50 mm
Mixture of PP and 5003RM5N
 V-2
@Thickness 3.00 mm
Mixture of PP and 5003RM5N

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPROCKS030 / 278538

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.