MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Matexcel MoS-029 MCM-41 Molecular Sieve
Categories: Other Engineering Material

Material Notes: MCM-41 molecular sieve is a long-range ordered mesoporous material with uniform pore size. It has the characteristics of extremely high BET specific surface area, large adsorption capacity and uniform mesoporous structure. , alkylation, olefin polymerization, separation of CO2 and CH4 and other acid catalysis fields and petrochemical separation processes have considerable potential application value, in heterogeneous catalysis, ion exchange, sensing technology, adsorption separation and advanced inorganic materials It also has high application value in other fields.

Morphology: Powder

Key Words: Synonyms: MCM-41 Molecular Sieve
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Product overviewSiO2/Al2O3(mol): =300 BET specific surface area: 350~800 Relative crystallinity(%): =90 Na2O(%): =0.1 Burn(%): =5 Pore size (nm): 2~5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMXCK2048 / 300679

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.