VESTAMID® L1930 black 9.7503 is a heat stabilized, with 30% milled glass fiber-reinforced PA 12 compound suitable for injection molding. Due to the reinforcement moldings from this compound exhibit a high strength and rigidity. Because PA 12 absorbs only little water, the parts have a good dimensional stability and almost unaffected mechanical properties at changing ambient humidity. Due to the reinforcement the shrinking of moldings is decreased compared with unreinforced compounds. Using specialty short glass fibers for the reinforcement of VESTAMID® L1930 black 9.7503 the difference between longitudinal and transverse shrinkage relating to the flow direction of the melt is significantly lower than with common glass fiber-reinforced products. Therefore especially low-warpage precision parts can be molded. As a semi-crystalline material VESTAMID® L1930 black 9.7503 feature an outstanding chemical resistance, e.g., against fuels, oils and fats. VESTAMID® L1930 black 9.7503 is supplied as cylindrical pellets in moisture-proof packaging. Property data for dry samples. Information provided by Evonik. |