Compound 3825 is an 80 cream colored Buna N elastomer, it is formulated with FDA sanctioned materials. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 BF 815 EO14 EO34; 6 BG 815 A14 EO14 EO34; 7 BG 815 EA14 EF11 EF21; 4 BK 815 A24 EF11 EO14 This Compound is RoHS Compliant Information provided by Pressure Seals Inc. |