MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Borealis LE0865 LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: LE0865 is a natural, modified polyethylene compound containing a mineral filler. It is especially designed for standstill or as a shutdown compound. LE0865 does not stick hard to metal surfaces and is therefore easy to remove by purging, or mechanically with e.g. a brass tool. The heat stability of the compound prevents thermal degradation that can result in oxidized particles that may be formed during extruder standstill. The compound has been demonstrated effective in allowing weekend shut down of film extrusion lines without dismantling for cleaning.
  • Does not stick hard to metal surfaces
  • Allowing weekend shut down of extrusion lines
  • Excellent heat stabilization
Applications: Purging and cleaning resin

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183-1
Melt Flow 1.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
Storage Temperature 10.0 - 30.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9804 / 323161

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.