High melt flow for injection molding, lubricated KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, ease of melt processing, high purity and excellent chemical resistance to organics, acids and bases. These properties make it well-suited for applications in healthcare, transportation, electronics, chemical processing and other industrial uses. KetaSpire® KT-880 NT can be easily processed using typical injection molding processes. This resin is also available as KT-880P in a natural-color coarse powder form for compounding. Pellets of KT-880 are supplied lightly dusted with the lubricant calcium stearate (0.01% level) to aid with pellet conveyance in plastication screws. The equivalent unlubricated natural color grade of high flow KetaSpire® is available as KT-880 NL. - Black: KT-880 BK 95 - Natural: KT-880 NT Markets/Uses: Aircraft / Mechanical & Structural Applications / Cable Ties; Aircraft / Mechanical & Structural Applications / Environmental Control System Components; Aircraft / Mechanical & Structural Applications / Handles; Aircraft / Mechanical & Structural Applications / Seals; Aircraft / Mechanical & Structural Applications / Spuds; Aircraft / Mechanical & Structural Applications / Stock Shapes for Prototyping; Films / High Temperature Films / Cable Ties; Films / High Temperature Films / Environmental Control System Components; Films / High Temperature Films / Handles; Films / High Temperature Films / Seals; Films / High Temperature Films / Spuds; Healthcare / Medical Devices / Case Handles and Brackets; Healthcare / Medical Devices / Dental Instruments; Healthcare / Medical Devices / Medical Pump Seals; Healthcare / Medical Devices / Medical Reusable; Healthcare / Medical Devices / Medical/Healthcare Applications; Healthcare / Medical Devices / Orthopedics; Healthcare / Medical Devices / Packaging, Rigid Medical; Healthcare / Medical Devices / Sizing Trials; Healthcare / Medical Devices / Surgical Instruments; Oil & Gas / Down Hole / Back-Up Seal Rings; Oil & Gas / Down Hole / Down Hole Connectors; Oil & Gas / Down Hole / Electrical Connectors; Oil & Gas / Down Hole / Labyrinth Seals; Oil & Gas / Down Hole / Motor End Plate Applications: Aircraft Applications; Connectors; Dental Applications; Electrical/Electronic Applications; Film; Hospital Goods; Industrial Applications; Medical Devices; Medical/Healthcare Applications; Oil/Gas Applications; Pump Parts; Seals; Surgical Instruments Features: Autoclave Sterilizable; Biocompatible; Chemical Resistant; Ductile; E-beam Sterilizable; Ethylene Oxide Sterilizable; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; Good Impact Resistance; Good Sterilizability; Heat Sterilizable; High Flow; High Heat Resistance; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam Sterilizable Information provided by Solvay Specialty Polymers. |