MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Amodel® AE-8935 PPA, 35% glass fiber for modern Auto E/E environments
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: Amodel AE-8935 is a 35% glycol resistant glass-reinforced heat stabilized polyphthalamide (PPA) resin designed to work in the modern automotive electrical environment. It is distinguished by a high heat deflection temperature, high flexural modulus, high tensile strength and low moisture absorption. This grade displays excellent resistance to cracks which may occur during thermal shock cycling.

- Black: AE-8935 BK902

Applications: Automotive Electronics; Connectors; Electrical Parts; Electrical/Electronic Applications

Features: Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Glycol Resistance; Good Stiffness; High Heat Resistance; High Stiffness; High Strength; High Temperature Strength; Low Moisture Absorption

Injection notes: Injection Rate: 3-4 inch/second (7.5-10 cm/sec)
Holding Pressure: 50% of injection pressure
Mold Temperature:
- Higher tool temperatures might be required for thin wall sections
Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³Method A; ISO 1183
Water Absorption at Saturation 0.16 %0.16 %ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 220 MPa31900 psiISO 527-2
Elongation at Break 2.4 %2.4 %ISO 527-2
Tensile Modulus 12.6 GPa1830 ksiISO 527-2
Flexural Strength 300 MPa43500 psiISO 178
Flexural Modulus 12.2 GPa1770 ksiISO 178
Charpy Impact Unnotched 9.60 J/cm²45.7 ft-lb/in²Type 1, Edgewise; ISO 179
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²Type 1, Edgewise, Notch A; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Comparative Tracking Index >= 600 V>= 600 VUL 746
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 290 °C554 °FUnannealed; ISO 75-2/A
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 310 - 330 °C590 - 626 °F
Middle Barrel Temperature 315 - 330 °C599 - 626 °F
Front Barrel Temperature 325 - 335 °C617 - 635 °F
Melt Temperature 320 - 345 °C608 - 653 °FInjection
Mold Temperature 150 °C302 °F
Drying Temperature 120 °C
@Time 14400 sec
248 °F
@Time 4.00 hour
Moisture Content 0.030 - 0.060 %0.030 - 0.060 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4072 / 279872

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.