Product Description: FRblend® PBT-1301 is a glass filled, flame retardant polybutylene -terephathalate compound. The flame retardant system is based on brominated aromatic which is used in thermoplastic systems. Features: - Good chemical resistance
- Excellent flame retardancy
- Heat stability
- Good mechanical properties
Uses:- Business machines
- Electrical/electronics components
- Automotive components
Forms:Processing Method:Information provided by Colour Image Plastic Compound Sdn Bhd |