MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMID® Care ML94 Medical Grade Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Medium viscosity, heat stabilized Polyamide 12 for medical application. VESTAMID® Care ML94 is resistant to body fluids and are toxicologically safe.

Features: High bursting strength; Flexible and reliable; High chemical resistance; Low sliding friction; High toughness; Good mechanical properties; Low processing tolerances.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
Water Absorption 1.5 %1.5 %Sim. to ISO 62
Moisture Absorption 0.800 %0.800 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inISO 294-4, 2577
Melt Flow 110 g/10 min
@Load 5.00 kg,
Temperature 275 °C
110 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 53.0 MPa7690 psiISO 527
Tensile Strength, Yield 45.0 MPa6530 psiISO 527
Elongation at Break >= 50 %>= 50 %Nominal; ISO 527
 265 %265 %ISO 527
Elongation at Yield 5.0 %5.0 %ISO 527
Tensile Modulus 1.44 GPa209 ksiISO 527
50% Modulus 33.0 MPa
@Strain 50 %
33.0 MPa
@Strain 50 %
ISO 527
Charpy Impact, Notched  0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
Complete Break; ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Complete Break; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 150 µm/m-°C
@Temperature 23.0 - 55.0 °C
83.3 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Melting Point 178 °C352 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75-1/-2
Vicat Softening Point 140 °C284 °FMethod B: 10 N, 50 K/h; ISO 306
 170 °C338 °FMethod A: 10 N, 50 K/h; ISO 306
Glass Transition Temp, Tg 45.0 °C113 °FISO 11357-1/-2
Flammability Test 1.0
@Thickness 1.60 mm
1.0
@Thickness 0.0630 in
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTAMID® X7293 Nylon 12, Extrusion/Tubing Grade
Evonik Vestamid® L2124 Plasticized Nylon 12
Evonik VESTAMID® E62-S1 Nylon 12 Elastomer
Evonik VESTAMID® DX9303 Nylon 612
Evonik VESTAMID® Care ME71 Medical Grade Nylon 12

PEVONIK827 / 243036

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.