MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Veradel® A-101 Polyethersulfone (PESU)
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: Veradel® A-101 is a very low melt flow general purpose amorphous PESU resin for extrusion and injection molding. This transparent grade offers high heat deflection temperature, excellent toughness and dimensional stability and resistance to mineral acids. Other desirable properties include thermal stability, creep resistance and inherent flame resistance. This grade was formerly marketed as Radel® A PESU.

- Natural: Veradel® A-101 NT

Applications: Film; Sheet; Tubing

Features: Acid Resistant; Creep Resistant; Flame Retardant; Food Contact Acceptable; Good Dimensional Stability; Good Thermal Stability; Good Toughness; Steam Resistant

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ASTM D792
Water Absorption 0.60 %
@Time 86400 sec
0.60 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inASTM D955
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 380 °C
13 g/10 min
@Load 4.76 lb,
Temperature 716 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 83.0 MPa12000 psiASTM D638
Elongation at Yield 6.5 %6.5 %ASTM D638
Tensile Modulus 2.60 GPa377 ksiASTM D638
Flexural Strength 111 MPa16100 psiASTM D790
Flexural Modulus 2.90 GPa421 ksiASTM D790
Izod Impact, Notched 0.850 J/cm1.59 ft-lb/inASTM D256
Tensile Impact Strength 336 kJ/m²160 ft-lb/in²ASTM D1822
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.70e+15 ohm-cm1.70e+15 ohm-cmASTM D257
Dielectric Constant  3.5
@Frequency 1000 Hz
3.5
@Frequency 1000 Hz
ASTM D150
 3.51
@Frequency 60 Hz
3.51
@Frequency 60 Hz
ASTM D150
 3.54
@Frequency 1e+6 Hz
3.54
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm381 kV/inASTM D149
Dissipation Factor  0.0017
@Frequency 60 Hz
0.0017
@Frequency 60 Hz
ASTM D150
 0.0022
@Frequency 1000 Hz
0.0022
@Frequency 1000 Hz
ASTM D150
 0.0056
@Frequency 1e+6 Hz
0.0056
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 49.0 µm/m-°C27.2 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 204 °C399 °FUnannealed; ASTM D648
UL RTI, Electrical 180 °C
@Thickness 0.800 mm
356 °F
@Thickness 0.0315 in
UL RTI, Mechanical with Impact 170 °C
@Thickness 0.800 mm
338 °F
@Thickness 0.0315 in
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Zone 1 327 - 371 °C621 - 700 °FExtrusion
Melt Temperature 343 - 390 °C649 - 734 °FExtrusion
Drying Temperature 177 °C
@Time 9000 sec
351 °F
@Time 2.50 hour
Extrusion
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
FormsPellets
ProcessingExtrusion; Film Extrusion; Sheet Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4601 / 280401

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.