MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Teflon™ 100 FEP Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP); Fluorinated Ethylene Propylene (FEP), Molded/Extruded

Material Notes: Teflon™ FEP 100 is a melt-processible copolymer of tetrafluoroethylene and hexafluoropropylene, without additives, that meets the requirements of ASTM D 2116 Type I. It offers the excellent combination of properties characteristic of Teflon™ fluoroplastic resins: non-aging characteristics, chemical inertness, exceptional dielectric properties, heat resistance, toughness and flexibility, low coefficient of friction, non-stick characteristics, negligible moisture absorption, low flammability, performance at temperature extremes, and excellent weather resistance. Teflon™ FEP 100 is a general-purpose grade and is used in many different applications. It can be melt-extruded, and is used for wire coating as primary insulation and, in certain cases, for cable jacketing. Cables insulated with Teflon™ FEP 100 have met the requirements of Underwriters Laboratory UL910 Steiner Tunnel tests for installation in plenums without metal conduits.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.14 g/ccASTM D792
Water Absorption <= 0.010 %
@Time 86400 sec
ASTM D570
Melt Flow 6.8 g/10 min
@Load 5.00 kg,
Temperature 372 °C
ASTM D2116
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 56ASTM D2240
Tensile Strength 26.0 MPaASTM D638
Elongation at Break 300 %ASTM D638
Flexural Modulus 0.586 GPaASTM D790
Flex Crack Resistance 10000
@Thickness 0.203 mm
Cycles MIT Folding Endurance; ASTM D2176
Izod Impact, Notched NBASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+18 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+16 ohmASTM D257
Dielectric Constant 2.03
@Frequency 1000 Hz
ASTM D150
 2.03
@Frequency 1e+9 Hz
ASTM D150
Dielectric Strength >= 80.0 kV/mm
@Thickness 0.250 mm
ASTM D149
Dissipation Factor 0.000070
@Frequency 1000 Hz
ASTM D150
 0.0010
@Frequency 1e+9 Hz
ASTM D150
Arc Resistance 300 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CASTM D3418
Maximum Service Temperature, Air 205 °CContinuous, per accelerated heat-aging test
Flammability, UL94 V-0
Oxygen Index >= 95 %ASTM D2863
 
Descriptive Properties
Chemical/Solvent ResistanceExcellentASTM D543
Critical Shear Rate (1/s)22Chemours Method. 372°C
Detergent Resistance (hours)480On grit blasted aluminum.
 600On aluminum
 744
Guide DDR Range for Cable Extrusion60-120
Heat of Combustion5.1 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)744+ASTM B117. 5% NaCl at 35 °C (95 °F).
Weather Resistance (years unaffected)20Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDU8785 / 268711

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.