MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Corning Med-X® X-Ray Shielding Glass
Categories: Ceramic; Glass

Material Notes: Med-X® Glass provides transparent and safe protective shielding against X-ray radiation for medical, technical, and research applications. Its high lead and barium content, and wide thickness range, provides shielding against radiation from equipment operating in the 80 to 300 kV range.

Corning Med-X Glass is compatible with a large range of installations and other viewing applications such as: Viewing windows for X-ray, angiography, CT scans; Screens for medical diagnostics; Protection windows/glove boxes in laboratories; Airport security X-ray screens; Lenses for safety goggles

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 409kg/mm²
Modulus of Elasticity 62.6 GPa
Poissons Ratio 0.36
Shear Modulus 24.8 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.88 µm/m-°C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.76nd
Transmission, Visible >= 85 %
@Wavelength >=55.0 nm,
Thickness 5.00 mm
 
Component Elements PropertiesOriginal ValueComments
Barium, Ba 17 %
Lead, Pb 52 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexWeb® HRH-327 - 3/16 - 5.0 Fiberglass Reinforced Polyimide Honeycomb
Titanium Carbide, TiC
Dicor Castable Fluormica Glass-Ceramic
Corning Large Cover Gorilla® Glass Touch Screen Glass
Corning Ba PC 588 Photochromic Barium Glass, Code 8082

CCORNG980 / 233276

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.