MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

ASI® MP 5405 NS Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: MP5405NS is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is a thixotropic paste consistency to prevent running and sagging. It gives good resistance to water, salt spray, inorganic acids and bases, and most organic solvents. It was formulated to a 1:1 mix ratio for use in either MMD equipment or side-by-side dual cartridges for easy dispensing.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity  1.15 g/cc
@Temperature 25.0 °C
1.15 g/cc
@Temperature 77.0 °F
part B
 1.16 g/cc
@Temperature 25.0 °C
1.16 g/cc
@Temperature 77.0 °F
mixed
 1.17 g/cc
@Temperature 25.0 °C
1.17 g/cc
@Temperature 77.0 °F
part A
Viscosity  1.50e+6 cP
@Temperature 25.0 °C
1.50e+6 cP
@Temperature 77.0 °F
part A
 1.50e+6 cP
@Temperature 25.0 °C
1.50e+6 cP
@Temperature 77.0 °F
part B
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80
@Temperature 25.0 °C
80
@Temperature 77.0 °F
Tensile Strength 48.3 MPa
@Temperature 25.0 °C
7000 psi
@Temperature 77.0 °F
Elongation at Break 3.0 - 5.0 %
@Temperature 25.0 °C
3.0 - 5.0 %
@Temperature 77.0 °F
Adhesive Bond Strength 19.3 MPa2800 psiLap Shear; Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 8.00e+14 ohm-cm
@Temperature 25.0 °C
>= 8.00e+14 ohm-cm
@Temperature 77.0 °F
Dielectric Constant 4.5
@Frequency 100 Hz,
Temperature 25.0 °C
4.5
@Frequency 100 Hz,
Temperature 77.0 °F
Dielectric Strength 16.1 kV/mm
@Temperature 25.0 °C
410 kV/in
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 62.0 µm/m-°C
@Temperature 25.0 °C
34.4 µin/in-°F
@Temperature 77.0 °F
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 3.00 - 5.00 min
@Temperature 25.0 °C
3.00 - 5.00 min
@Temperature 77.0 °F
20 grams
 
Descriptive Properties
Color / appearancetranslucent/white
ViscosityMixed, non-sag paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASINC9082 / 233449

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.