MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow Affinity™ PF 1162G Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description:
  • For food packaging
  • Excellent seal flexibility and strength properties
Complies with: US FDA 21 CFR 175.105; Consult the regulations for complete details

Availability: Latin America; North America

Additive: Antiblock: 5000 ppm; Processing Aid: No; Slip: 2500 ppm

Agency Ratings: FDA FCN 424

Form: Pellets

Processing Method: Blown Film

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.902 g/ccASTM D792
Mooney Viscosity 19
@Temperature 121 °C
ML 1+4; ASTM D1646
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 5000 ppm
Slip Level 2500 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 861 psi
@Thickness 0.0508 mm
ASTM D882
Film Tensile Strength at Yield, TD 838 psi
@Thickness 0.0508 mm
ASTM D882
Film Elongation at Break, MD 610 %
@Thickness 0.0508 mm
ASTM D882
Film Elongation at Break, TD 650 %
@Thickness 0.0508 mm
ASTM D882
Elmendorf Tear Strength MD 400 g0.002; ASTM D1922
Elmendorf Tear Strength TD 510 g0.002; ASTM D1922
Dart Drop Test >= 850 g
@Thickness 0.0508 mm
ASTM D1709A
Film Tensile Strength at Break, MD 6410 psi
@Thickness 0.0508 mm
ASTM D882
Film Tensile Strength at Break, TD 6040 psi
@Thickness 0.0508 mm
ASTM D882
Heat Seal Strength Initiation Temperature 176 °FASTM D1525
 
Thermal PropertiesOriginal ValueComments
Melting Point 203 °F
Vicat Softening Point 169 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 5.0 %
@Thickness 0.0508 mm
ASTM D1003
Gloss 81 %
@Thickness 0.0508 mm
45°, Cast Film; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 350 - 450 °F
Blow-up Ratio (BUR) 2.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF377 / 311070

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.