MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Mackine® 301 Flake Surfactant  (discontinued **)
Categories: Fluid

Material Notes: Standard Applications: Mackine 301 Flake is fatty amido-functional tertiary amine available in an easy to handle flake form. It can be a high purity, vegetable derived grade of stearic acid with a minimum of 90% C-18 content. Mackine 301 Flake provides the major conditioning action for a crème rinse, finishing rinse or conditioner. The major conditioning action for a crème rinse, finishing rinse or conditioner. The major advantage the amine salts offer over quaternary ammonium compounds is that they can be rinsed more easily from the hair. Thus reducing the possibility of surfactant buildup. When blended with the proper co-emulsifier, e.g cetyl alcohol, PEG 400 distearate, both pearly or opaque type conditioners can be developed.

Chemical Name: Stearamidopropyl Dimethylamine

CAS No: 7651-02-7

EINEC Number: 231-609-1

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/cc
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 4.0200A
 
Thermal PropertiesOriginal ValueComments
Melting Point 61.0 - 70.0 °CFisher Johns; 136A
 65.0 - 69.0 °CCapillary; 134A
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 5.0104A
 
Processing PropertiesOriginal ValueComments
Shelf Life 48.6 Month
 
Descriptive Properties
AppearanceClear to hazy liquid100P
 Waxy Flake100C
Content<0.3%DMAPA
 148-152Amine Number, 208A

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLVAY747 / 218475

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.