MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Persian Gulf Polymer PP-EP548T Block Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: EP548 is a high melt flow rate, nucleated heterophasic copolymer with a special antistatic additive used for thin-walled injection molding. IML and houseware applications. It has improved balance of mechanical properties. The use of EP548T allows high productivity due to the easy mold filling and short cycle times. In comparison with conventional copolymers with the same MFR and the same toughness, EP548T exhibits 15% higher rigidity. EP548T is suitable for food contact.

Processing Method: Injection molding.

Features: High fluidity, Easy mold filling and short cycle times, Desirable impact/ stiffness balance, antistatic properties, Heterophasic copolymer.

Typical Applications: TWIM/IML food containers (Margarine yogurt, soft cheese, pudding, etc.), housewares, Caps and closures, Flower pots and cool boxes, Sport, leisure and toys.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ASTM D785
Tensile Strength, Yield 28.0 MPaASTM D638
Elongation at Yield 5.0 %ASTM D638
Flexural Modulus 1500 MPaASTM D790
Izod Impact, Notched 30.0 J/m
@Temperature -20.0 °C
ASTM D256
 60.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °CASTM D648
Vicat Softening Point 151 °C
@Load 1.02 kg
ASTM D1525
 
Descriptive Properties
Accelerated Oven Aging360 hrsIn air @ 150°C. ASTM D3012

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPERSI983 / 250387

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.