MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Arla ATECH® 3400 ABS Sheet
Categories: Polymer; Thermoset; Phenolic

Material Notes: ATECH is a series of sheets based on ABS which is a raw material with very high impact-strength. ABS also has impressive thermal qualities and is easy to thermoform and fabricate. The ATECH 3400 is a super high impact ABS with a matte colored PMMA top layer.
Also Available In: ATECH 3400GC Gloss control range with a gloss level to meet specific requirements; ATECH 3440 with matte PMMA surface both sides
Recycling: The total recycling concept (TRC) covers all types of sheets to provide cost savings. Off-cuts from the sheets can be used in production of new sheets by co-extruding virgin material as the top layer. Care is taken that all quality requirements are met.

Benefits: Easy to thermoform; High impact strength; Good thermal qualities

Application: The great weathering properties and gloss characteristics makes ATECH 3400 series suitable for both indoor and outdoor applications. For example; advertising, building & construction, industrial machines, automotive etc.

Information provided by Arla Plast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccISO 1183
Linear Mold Shrinkage 0.0060 - 0.0070 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 33.0 MPaISO 527
Elongation at Break 55 %ISO 527
Tensile Modulus 1.90 GPaISO 527
Izod Impact, Notched (ISO) 20.0 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
@Temperature -35.0 °C
ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °CISO 75-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARLA905 / 301083

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.