MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ascend Performance Materials Starflam® FR350J NT0727 PA66 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Starflam FR350J NT0727 is an unreinforced, halogenated flame-retardant PA66 compound designed with excellent glow wire ignition temperature (GWIT). It exhibits excellent strength and ductility, allowing increased flexibility in product design needed for living hinges and snap fits. FR350J NT0727 provides enhanced flow and is lubricated for machine feed and easy mold release.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³DAM; ISO 1183
Water Absorption 0.90 %
@Time 86400 sec
0.90 %
@Time 24.0 hour
DAM; ISO 62
Moisture Absorption at Equilibrium 1.8 %1.8 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.014 cm/cm
@Thickness 2.00 mm
0.014 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.017 cm/cm
@Thickness 2.00 mm
0.017 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 47.0 MPa6820 psi50% RH; ISO 527-2
 69.0 MPa10000 psiDAM; ISO 527-2
Tensile Strength, Yield 75.0 MPa10900 psiDAM; ISO 527-2
Elongation at Break 22 %22 %DAM; ISO 527-2
 64 %64 %50% RH; ISO 527-2
Elongation at Yield 4.0 %4.0 %DAM; ISO 527-2
Tensile Modulus 1.70 GPa247 ksi50% RH; ISO 527-2
 3.40 GPa493 ksiDAM; ISO 527-2
Flexural Strength 37.0 MPa5370 psi50% RH; ISO 178
 98.0 MPa14200 psiDAM; ISO 178
Flexural Modulus 1.50 GPa218 ksi50% RH; ISO 178
 3.60 GPa522 ksiDAM; ISO 178
Poissons Ratio 0.380.38ISO 527-2
Izod Impact, Notched (ISO)  3.80 kJ/m²
@Temperature 23.0 °C
1.81 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 4.20 kJ/m²
@Temperature -40.0 °C
2.00 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 4.40 kJ/m²
@Temperature -30.0 °C
2.09 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 4.50 kJ/m²
@Temperature -30.0 °C
2.14 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 4.60 kJ/m²
@Temperature -40.0 °C
2.19 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 180/1A
 5.80 kJ/m²
@Temperature 23.0 °C
2.76 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact, Notched  0.320 J/cm²
@Temperature -30.0 °C
1.52 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.330 J/cm²
@Temperature -40.0 °C
1.57 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eA
 0.330 J/cm²
@Temperature -30.0 °C
1.57 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 0.340 J/cm²
@Temperature 23.0 °C
1.62 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 0.350 J/cm²
@Temperature -40.0 °C
1.67 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 0.610 J/cm²
@Temperature 23.0 °C
2.90 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  3.50e+11 ohm-cm
@Thickness 1.00 mm
3.50e+11 ohm-cm
@Thickness 0.0394 in
50% RH; IEC 60093
 2.80e+15 ohm-cm
@Thickness 1.00 mm
2.80e+15 ohm-cm
@Thickness 0.0394 in
DAM; IEC 60093
Hot Wire Ignition, HWI >= 120 sec>= 120 secPLC 0; UL 746
 >= 120 sec>= 120 secPLC 0; UL 746
 >= 120 sec>= 120 secPLC 0; UL 746
 >= 120 sec>= 120 secPLC 0; UL 746
High Amp Arc Ignition, HAI >= 120 arcs>= 120 arcsPLC 0; UL 746
 >= 120 arcs>= 120 arcsPLC 0; UL 746
 >= 120 arcs>= 120 arcsPLC 0; UL 746
 >= 120 arcs>= 120 arcsPLC 0; UL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
33.3 µin/in-°F
@Thickness 0.0787 in,
Temperature 95.0 - 131 °F
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 62.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
34.4 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
DAM; ISO 11359-2
Melting Point 265 °C509 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 209 °C408 °FUnannealed; 50% RH; ISO 75-2/B
 218 °C424 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C174 °FUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical  130 °C
@Thickness 0.400 mm
266 °F
@Thickness 0.0157 in
UL 746
 130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746
 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL 746
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  65.0 °C
@Thickness 0.400 mm
149 °F
@Thickness 0.0157 in
UL 746
 65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL 746
 65.0 °C
@Thickness 1.50 mm
149 °F
@Thickness 0.0591 in
UL 746
 65.0 °C
@Thickness 3.00 mm
149 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  110 °C
@Thickness 0.400 mm
230 °F
@Thickness 0.0157 in
UL 746
 110 °C
@Thickness 0.750 mm
230 °F
@Thickness 0.0295 in
UL 746
 110 °C
@Thickness 1.50 mm
230 °F
@Thickness 0.0591 in
UL 746
 110 °C
@Thickness 3.00 mm
230 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  V-0
@Thickness 0.200 mm
V-0
@Thickness 0.00787 in
 V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 5VA
@Thickness 1.50 mm
5VA
@Thickness 0.0591 in
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
Glow Wire Ignition Temperature  960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
IEC 60695-2-13
 960 °C
@Thickness 0.750 mm
1760 °F
@Thickness 0.0295 in
IEC 60695-2-13
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-13
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
IEC 60695-2-12
 960 °C
@Thickness 0.750 mm
1760 °F
@Thickness 0.0295 in
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 290 °C500 - 554 °FInjection
Middle Barrel Temperature 260 - 290 °C500 - 554 °FInjection
Front Barrel Temperature 260 - 290 °C500 - 554 °FInjection
Nozzle Temperature 260 - 290 °C500 - 554 °FInjection
Melt Temperature 270 - 285 °C518 - 545 °FInjection
Mold Temperature 65.0 - 95.0 °C149 - 203 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Lubricant
Agency RatingsRoHS Compliant
AppearanceNatural Color
FeaturesChemical Resistant
 Corrosion Resistant
 Flame Retardant
 Good Electrical Properties
 Good Mold Release
 Halogenated
 Heat Aging Resistant
 Homopolymer
 Ignition Resistant
 Lubricated
 Organic Heat Stabilized
 Thermal Stability
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific
UL File NumberE70062

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE9117 / 287568

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.