MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

EMS-Grivory Grilamid® 2S 25 W 20 HL X nat Nylon 6/10, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Plasticizer

Features: Good Flexibility; High Heat Resistance; High Impact Resistance; High Viscosity; Plasticized; Renewable Resource Content

Uses: Automotive Applications; Electrical/Electronic Applications; Hydraulic Applications; Pneumatic Applications; Profiles; Tubing; Wire & Cable Applications

Appearance: Natural Color

Forms: Granules

Processing Method: Extrusion; Profile Extrusion

Information provided by EMS-Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ISO 1183
Water Absorption 0.50 %0.50 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 3.0 %3.0 %ISO 62
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.018 cm/cm0.018 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 50.0 MPa7250 psiISO 2039-1
Tensile Strength at Break 50.0 MPa7250 psiISO 527-2
Elongation at Break >= 50 %>= 50 %ISO 527-2
Tensile Modulus 0.752 GPa109 ksiISO 527-1
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.49 J/cm²
@Temperature -30.0 °C
7.10 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 198 µm/m-°C110 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 149 µm/m-°C83.0 µin/in-°FISO 11359-2
Melting Point 215 °C419 °F10ºC/min; ISO 11357-3
Maximum Service Temperature, Air 108 °C226 °FLong Term; ISO 2578
 170 °C338 °FShort Term
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FUnannealed; ISO 75-2/A
Flammability, UL94 HB
@Thickness 0.762 mm
HB
@Thickness 0.0300 in
IEC 60695-11-10,-20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRIM022 / 307381

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.