MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Pocan® DP 2004 000000 PBT  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Flame Retardant; Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: PBT, non-reinforced, injection molding, halogen free flame retardant

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0023 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0023 cm/cmISO 294-4, 2577
Melt Flow 82 g/10 min
@Load 2.16 kg,
Temperature 250 °C
Estimated using room temperature density; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 53.0 MPaISO 527-1/-2
Tensile Strength, Yield 55.0 MPaISO 527-1/-2
Elongation at Break 20 %ISO 527-1/-2
Elongation at Yield 8.0 %ISO 527-1/-2
Tensile Modulus 2300 MPaISO 527-1/-2
Charpy Impact Unnotched 85.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Strength 30.0 kV/mmIEC 60243-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 120 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°CISO 11359-1/-2
Melting Point 224 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 163 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 48.0 °CISO 75-1/-2
Flammability, UL94 V-2
@Thickness 0.750 mm
IEC 60695-11-10
 V-2
@Thickness 1.50 mm
IEC 60695-11-10
Oxygen Index 28 %ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °CInjection Molding; ISO 294
Mold Temperature 80.0 °CInjection Molding; ISO 10724
 
Descriptive Properties
AdditivesFlame retarding agent
FeaturesFlame retardant
FormPellets
ISO Short NameISO 7792-1-PBT,GFHMR,09-020; ISO 1043-PBT FR(30+40)
ProcessingInjection molding
RegionAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANX0877 / 99092

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.