MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polyrocks Chemical 4000RMP55 Polyamide master batches
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Polyamide master batches is halogen free environmental flame retardant master batches with PA6 as carrier, concentration of 55% MCA, which specially used for non-filled, non-reinforced polyamide material. Carbonize, expansion and physical cooling mechanism of MCA play the flame retardant performance. Halogen-free flame retardant master batches flammability reach UL94V-0, glow wire test meets GWIT750? and GWFI960?. It has the characteristics of low density, great electrical property, no smoke and no corrosion to molds etc.

Information provided by Polyrocks

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccASTM D792
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-2PA66/PA6, 4000RMP55: 10-17%
 V-25-30%MF PA66/PA6, 4000RMP55: 10-25%
 V-25-30%GF PA66/PA6, 4000RMP55: 10-27%
 V-0PA66, 4000RMP55: 23-25%
 V-0PA6, 4000RMP55: 25-27%
Glow Wire Ignition Temperature 750 °CIEC60695-2-13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPROCKS033 / 278541

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.