MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Petropol Durepol® A3 G30 UV PRTA011 BT304 PBT, 30% Glass Fiber Reinforced, UV Stabilized
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Resin ID (ISO 1043): PBT
Color: Black
Processing: Injection Molding

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.53 g/cc0.0553 lb/in³ISO 1183
Water Absorption 0.10 - 0.20 %0.10 - 0.20 %Equilibrium; ISO 62
 0.40 %
@Time 86400 sec
0.40 %
@Time 24.0 hour
Immersion; ISO 62
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 - 0.0090 cm/cm0.0050 - 0.0090 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 110 MPa16000 psiISO 527-1-2
Elongation at Yield 2.5 %2.5 %ISO 527-1-2
Tensile Modulus 9.67 GPa1400 ksiISO 527-1-2
Flexural Strength 200 MPa29000 psiISO 178
Flexural Modulus 9.05 GPa1310 ksiISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Dielectric Strength 17.0 kV/mm
@Thickness 3.00 mm
432 kV/in
@Thickness 0.118 in
ASTM D149
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °F
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75-1-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75-1-2
Vicat Softening Point  215 °C
@Load 5.10 kg
419 °F
@Load 11.2 lb
120°C/h; ISO 306
 220 °C
@Load 1.02 kg
428 °F
@Load 2.25 lb
120°C/h; ISO 306
UL RTI, Electrical  130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746
 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL 746
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746
 130 °C
@Thickness 6.00 mm
266 °F
@Thickness 0.236 in
UL 746
UL RTI, Mechanical with Impact  130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746
 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL 746
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746
 130 °C
@Thickness 6.00 mm
266 °F
@Thickness 0.236 in
UL 746
UL RTI, Mechanical without Impact  130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746
 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL 746
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746
 130 °C
@Thickness 6.00 mm
266 °F
@Thickness 0.236 in
UL 746
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 230 - 250 °C446 - 482 °FMolding
Mold Temperature 60.0 - 120 °C140 - 248 °F
Drying Temperature 80.0 - 120 °C176 - 248 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPETROPOL005 / 312913

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.