MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Starflam® 909 Nylon PA66/6-GF25 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: Starflam 909 (formerly Vydyne® 909) is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccDAM; ISO 1183
Water Absorption 0.70 %
@Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.3 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 90.0 MPa50% RH; ISO 527-2
 132 MPaDAM; ISO 527-2
Elongation at Break 2.2 %DAM; ISO 527-2
 3.0 %50% RH; ISO 527-2
Tensile Modulus 7100 MPa50% RH; ISO 527-2
 9100 MPaDAM; ISO 527-2
Flexural Strength 140 MPa50% RH; ISO 178
 193 MPaDAM; ISO 178
Flexural Modulus 5000 MPa50% RH; ISO 178
 8300 MPaDAM; ISO 178
Poissons Ratio 0.40ISO 527-2
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Charpy Impact Unnotched 35.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 40.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 9.40 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 9.50 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 60 - 120 sec
@Thickness 3.00 mm
PLC 6; ASTM D 495
Hot Wire Ignition, HWI >= 120 secPLC 0; UL 746
 >= 120 secPLC 0; UL 746
High Amp Arc Ignition, HAI >= 120 arcsPLC 0; UL 746
 >= 120 arcsPLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minPLC 3; UL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 250 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 250 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 230 °CUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical 130 °C
@Thickness 0.750 mm
UL 746
 130 °C
@Thickness 1.50 mm
UL 746
 130 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 0.750 mm
UL 746
 95.0 °C
@Thickness 1.50 mm
UL 746
 95.0 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 110 °C
@Thickness 0.750 mm
UL 746
 110 °C
@Thickness 1.50 mm
UL 746
 110 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-0
@Thickness 0.400 mm
 V-0
@Thickness 0.750 mm
 V-0
@Thickness 1.50 mm
 V-0
@Thickness 3.00 mm
 5VA
@Thickness 1.50 mm
 5VA
@Thickness 3.00 mm
Glow Wire Ignition Temperature 750 °C
@Thickness 0.750 mm
IEC 60695-2-13
 750 °C
@Thickness 1.50 mm
IEC 60695-2-13
 800 °C
@Thickness 3.00 mm
IEC 60695-2-13
 930 °C
@Thickness 0.400 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.400 mm
IEC 60695-2-12
 960 °C
@Thickness 0.750 mm
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 240 - 270 °CInjection
Middle Barrel Temperature 240 - 270 °CInjection
Front Barrel Temperature 240 - 270 °CInjection
Nozzle Temperature 240 - 270 °CInjection
Melt Temperature 250 - 270 °CInjection
Mold Temperature 65.0 - 95.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 hourInjection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Lubricant
AppearanceNatural Color
FeaturesCrack Resistant
 Flame Retardant
 Good Mold Release
 Good Toughness
 Halogenated
 High Rigidity
 High Strength
 Ignition Resistant
 Lubricated
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific
UL File NumberE70062

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE8700 / 293361

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.