MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Zortrax Z-ABS 2 Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer

Material Notes: Z-ABS is a versatile and economic material which perfectly matches the needs of users who begin their work with 3D printing as well as professionals who want to make savings on in-house prototyping. With a wide selection of post-processing methods, either mechanical or chemical, Z-ABS becomes well-suited not only for producing affordable prototypes, but also for creative applications, such as conceptual models, gadgets or figurines. Z-ABS is something you seek for if you need to 3D print low-cost, attractive-looking objects or prototypes with functional requirements.

Information provided by Zortrax

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183/B
Melt Flow 15 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 45.0 MPaISO 527-2
Elongation at Break 2.5 %
@Thickness 3.20 mm
ISO 527-2
Tensile Modulus 2300 MPaISO 527-2
Izod Impact, Notched (ISO) 9.00 kJ/m²ISO 180/A
Izod Impact, Unnotched (ISO) 19.0 kJ/m²ISO 180/A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 100 °CAnnealed; ISO 75-2/A
Vicat Softening Point 97.0 °C
@Load 5.00 kg
50° C/h; ISO 306/B50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZORT002 / 281881

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.