MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond Supreme 62-1 Two component epoxy resin system
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Convenient handling, long open time
  • Cures rapidly at moderately elevated temperatures
  • Superb physical strength profile
  • Good toughness
Master Bond Supreme 62-1 is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a very forgiving 100 to 10 mix ratio by weight. The pot life of 100 grams is greater than 12 hours. Typical cure schedules range from 4-6 hours at 140-158°F [60-70°C], 20-40 minutes at 176- 212°F [80-100°C] or 10-20 minutes at 257°F [125°C]. To obtain optimum properties, post curing at 212-302°F [100-150°C] for 2-4 hours is recommended. Following an optimum cure schedule, Supreme 62-1 has a glass transition temperature in the range of 155-160°C. Also noteworthy is its outstanding chemical resistance to acids, bases, many solvents and other chemicals, even at elevated temperatures. This system has excellent electrical insulation properties. Most noteworthy is that Supreme 62-1 is a toughened system with an enhanced ability to withstand thermal cycling. The service temperature range is -60°F to +450°F The color of Part A is clear and Part B is dark brown in color. Supreme 62-1 is a worthy candidate for aerospace, electronic, optical, specialty OEM and related applications, particularly when high temperature resistance, a degree of toughness and the ability to withstand aggressive chemicals is required.

Product Advantages:

  • Easy to use, very forgiving 100 to 10 mix ratio by weight (will fully cure using 100 to 5 mix ratio)
  • Impressively long working life
  • First rate electrical insulation properties
  • Protection from many aggressive chemicals
  • Versatile curing schedules
  • Outstanding dimensional stability
  • Meets NASA low outgassing specifications

Information provided by Masterbond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 50 - 500 cPPart B
 15000 - 25000 cPmixed
 30000 - 40000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75 - 85
Tensile Strength 8000 - 9000 psi
Elongation at Break 5.0 - 10 %
Tensile Modulus 450000 - 500000 psi
Adhesive Bond Strength 2000 - 2200 psilap shear, Al/Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 4.2
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -60.0 °F
Glass Transition Temp, Tg 155 - 160 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 4.00 hour
@Temperature 100 - 150 °C
Optimum post cure
 4.00 - 6.00 hour
@Temperature 60.0 - 70.0 °C
 10.0 - 20.0 min
@Temperature 125 °C
 20.0 - 40.0 min
@Temperature 80.0 - 100 °C
Working Life >= 720 minAfter mixing, 100 g batch
Shelf Life 12.0 MonthIn original unopened containers
 
Descriptive Properties
Mixing Ratio100:10Parts A to B, by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTM732 / 233789

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.