20% glass fiber, opaque, high melt flow for injection molding Veradel® AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resistance of the material, while maintaining most of its other basic characteristics. The combination of structural properties and cost effectiveness make this resin an attractive alternative to metals in many engineering applications. This grade was formerly marketed as Radel® A PESU - Natural: Veradel® AG-320 NT - Black: Veradel® AG-320 BK 184 Markets/Uses: Automotive / Automotive E/E / Engine Sensors; Automotive / Automotive E/E / Sensors Applications: Appliance Components; Appliances; Automotive Electronics; Batteries; Business Equipment; Electrical Parts; Electrical/Electronic Applications; Food Service Applications; Industrial Applications; Metal Replacement; Microwave Cookware; Plumbing Parts; Valves/Valve Parts Features: Acid Resistant; Chemical Resistant; Creep Resistant; Flame Retardant; Food Contact Acceptable; Good Adhesion; Good Dimensional Stability; Good Strength; Good Thermal Stability; Good Toughness; High Heat Resistance; High Rigidity; High Tensile Strength; Hydrolysis Resistant; Medium Flow; Medium Molecular Weight Information provided by Solvay Specialty Polymers. |