MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ITW Irathane Futura® ULTRACHROME 1552 Cross Linking Agent
Categories: Polymer; Thermoset

Material Notes: A cross linker used as an additive to Ultra chrome 452 when there is a requirement for increased adhesion. This would typically arise when the Ultra chrome 452 is being applied onto old 5410 or there is a time delay in production between Ultra thane 5410 and Ultra chrome 452 over coating.

RECOMMENDED APPLICATIONS: Only to be used with Ultra chrome 452.

FEATURES: • Specifically for use with Ultra chrome 452 as a cross linker to increase adhesion.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 50 %
 
Thermal PropertiesOriginal ValueComments
Flash Point 114.8 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 22.0 °C
In original unopened container in dry environment.
 
Descriptive Properties
Colorclear, colorless

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWI9236 / 239745

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.