Appearance: Amber Product Benefits: Cure: Heat cureApplication: Assembly LOCTITE ABLESTIK 5020 glass supported adhesive film is a higher purity version of ABLEFILM 550 adhesive film. It is designed for substrate attach and sealing microelectronic packages. This adhesive film meets the requirements of MIL-STD-883, Method 5011. Information provided by Loctite® |