Compound 19513 is a 50 durometer white colored Silicone elastomer. It exhibits good resistance to heat and compression set and it will remain non brittle at very low temperatures. It is formulated with FDA sanctioned materials. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 3 GE 504 A19 B37 EO16 EO36 F19 EA14; 4 GE 507 A19 B37 EO16 EO36 F19 EA14; 5 GE 507 A19 B37 EO16 EO36 F19 EA14 ZZ-R-765 Class 2a & 2b Grade 50 A-A-59588 Class 2a & 2b Grade 50 AMS 3302 3-A Sanitary Standards No. 18-03 Class IV Information provided by Pressure Seals Inc. |