Description: Thixotropic two-part epoxy adhesive. Its viscosity allows to be used for bonding, potting, filling and fairing applications. Features: - Room temperature cure (= 18oC/64oF)
- Outstanding mechanical properties over a wide range of temperature (-55oC/-67oF to 180oC/356oF)
- Suitable for random repair, non-metallic filler
Information provided by Hexcel Corporation. |