MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Molykote® G-4500 Multi-Purpose Synthetic Grease
Categories: Fluid; Lubricant; Aluminum Gellant; Polyalphaolefin (PAO)

Material Notes: Former Dow Corning product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.840 g/cc
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 314 kg
Four Ball Wear 0.500 mmscar size
Penetration P(60), 1/10 mm 280
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 325 °FContinuous
Minimum Service Temperature, Air -60.0 °F
 
Descriptive Properties
Bleed2.5%at 212°F
Dn Value325000
Drop Point520°F
Evaporation0.2%at 212°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nye Lubricants 734A-MS (RL) Synthetic Oil
Mitsubishi Chemical Advanced Materials Fluorosint® 500 PTFE, synthetic mica-filled PTFE, compression molded (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers (ASTM Product Data Sheet)
RTP Company RTP 1001 GB 15 TFE 5 Polybutylene Terephthalate (PBT), Glass Fiber - Glass Bead - PTFE Lubricated
RTP Company RTP 1001 TFE 15  Polybutylene Terephthalate (PBT) Glass Fiber 10% - PTFE 15%

PDOWC32 / 30748

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.