MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ RF0039S PA 66 (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LNP THERMOCOMP* RF0039S is a compound based on Nylon 66 resin containing 15% Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized.

Information provided by SABIC Innovative Plastics for the Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 g/ccISO 1183
 1.487 g/ccASTM D 792
Moisture Absorption 0.490 %
@Time 86400 sec
50% RH; ASTM D 570
Linear Mold Shrinkage, Flow 0.0089 cm/cm
@Time 86400 sec
ISO 294
 0.0090 cm/cm
@Time 86400 sec
ASTM D 955
Linear Mold Shrinkage, Transverse 0.0129 cm/cm
@Time 86400 sec
ISO 294
 0.013 cm/cm
@Time 86400 sec
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 98.0 MPaISO 527
 100 MPaASTM D 638
Elongation at Break 2.9 %ISO 527
 3.0 %ASTM D 638
Tensile Modulus 6060 MPa50 mm/min; ASTM D 638
 6300 MPa1 mm/min; ISO 527
Flexural Strength 160 MPaASTM D 790
 164 MPaISO 178
Flexural Modulus 600 MPaISO 178
 5170 MPaASTM D 790
Izod Impact, Notched 42.0 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Unnotched 523 J/m
@Temperature 23.0 °C
ASTM D 4812
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1U
Impact Test 1.00 JMultiaxial Impact; ISO 6603
Instrumented Impact Energy at Peak 5.00 J
@Temperature 23.0 °C
ASTM D 3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 251 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 219 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 226 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
Flammability, UL94 V-0
@Thickness 1.70 mm
UL 94 by SABIC-IP

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI47085 / 188170

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.