MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ ELCRIN™ 61000IiQ Polycarbonate + PBT (PC+PBT)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: LNP ELCRIN 61000IiQ compound is based on Polycarbonate / Polybutylene Terephthalate (PC/PBT) blend utilizing ELCRIN iQ upcycling technology containing minimum 22% Post-Consumer Recycling (PCR) weight content. Added features of this grade include: Impact Modified, Excellent Low Temperature Impact, Chemical Resistant, Colorable.

Features: Post-Consumer Recycled (PCR) content,Enhanced Low Temperature Impact,Chemical Resistance,Colorable,High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Density 1.20 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.0800 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.30 %ISO 62-1
Viscosity 12 cP
@Load 5.00 kg,
Temperature 250 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 46.0 MPa50 mm/min; ASTM D638
 47.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 45.0 MPa50 mm/min; ASTM D638
 49.0 MPa50 mm/min; ISO 527
Elongation at Break 140 %50 mm/min; ASTM D638
 150 %50 mm/min; ISO 527
Elongation at Yield 4.0 %50 mm/min; ASTM D638
 4.0 %50 mm/min; ISO 527
Tensile Modulus 1950 MPa1 mm/min; ISO 527
 2050 MPa50 mm/min; ASTM D638
Flexural Strength 70.0 MPayield, 2 mm/min; ISO 178
 74.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1920 MPa2 mm/min; ISO 178
 2000 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 650 JASTM D256
 600 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 55.0 kJ/m²80*10*4; ISO 180/1A
 47.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 55.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 50.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E831
 90.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 95.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E831
 95.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 75.0 °CUL 746B
UL RTI, Mechanical with Impact 75.0 °CUL 746B
UL RTI, Mechanical without Impact 75.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 250 - 265 °C
Zone 2 245 - 265 °C
Zone 3 250 - 270 °C
Melt Temperature 255 - 275 °CInjection Molding
Mold Temperature 40.0 - 90.0 °C
Drying Temperature 110 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 50 - 80 %
Vent Depth 0.00130 - 0.00200 cm
Screw Speed 40 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80604 / 288551

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.