MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Protective Coating PC-Wood Guardian™ Wood Preservative
Categories: Other Engineering Material

Material Notes: PC-Wood Guardian™ isused in preventing and controlling decay fungi. It is an effective treatment for wood and wood composite to kill and prevent infestations of decay fungi including white and brown rot and wet rot.

It is also effective for the prevention and control of wood destroying insects including, but not limited to, Subterranean Termites, Drywood Termites, Dampwood Termites, Powderpost Beetles, Deathwatch and Furniture Beetles, Carpenter Ants and Bark and Timber Beetles.

Application is usually made by mixing with water. It may also be used as a powder and dusted onto wood or wood composites.

Data provided by the manufacturer.

Key Words: PC Epoxy
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Bulk Density 0.320 - 0.480 g/cc
Solubility in Water 9.7 %
@Temperature 20.0 °C
 34.3 %
@Temperature 50.0 °C
pH 7.610% solution
 8.33% solution
 
Thermal PropertiesOriginal ValueComments
Melting Point 815 °C
 
Descriptive Properties
CAS Number of Main Component12280-03-4
ColorWhite
ConsistencyFine Powder
Main componentDisodium Octaborate Tetrahydrate (98%)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron LiquidWood® Deep Penetrating Wood Consolidant
Carbon-Core 13 mm+2.7 mm Lauan both sides Luan/Meranti Plywood Panels
Carbon-Core Carbon Balsa Wood
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Protective Coating PC-Rot Terminator® Epoxy Wood Consolidant

PEPXP90 / 124695

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.