Base Polymer: Polypropylene Heterophasic Copolymer Filler/Additive System: 20% Chalk, 10% Talcum Special Features: Heat ageing stabilization Market Segment: Various Application Area: Domestic appliances, gardening tools Typical Applications: Housings Information provided by Albis Plastics |