MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Corning XDF LIGHT GRAY Tinted Photochromic Glass
Categories: Ceramic; Glass; Optical

Material Notes: Application : Pretinted 77% photochromic glass suited for general or special purpose Tinted glasses. Neutral gray with excellent color rendition. Pass cited standards for traffic signal recognition at 2 mm thickness. Blanks for corrective lenses available on request.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.41 g/cc
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.35 µm/m-°C
@Temperature 20.0 - 300 °C
Softening Point 665 °C
Annealing Point 495 °C
Strain Point 665 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.523
@Wavelength 587.6 nm
Line: d; Helium
Abbe Number 56.7vd
Transmission, Visible 25 %
@Wavelength 380 - 780 nm,
Thickness 2.00 mm
Luminous, Darkened
 25 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
Blue light transmission factor, Darkened
 75 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
Blue light transmission factor, Faded
 77 %
@Wavelength 380 - 780 nm,
Thickness 2.00 mm
Luminous, Faded
UV Transmittance <= 0.10 %
@Thickness 2.00 mm
Solar UV-B transmission factor, Faded
 <= 0.10 %
@Thickness 2.00 mm
Solar UV-B transmission factor, Darkened
 2.0 %
@Thickness 2.00 mm
Solar UV-A transmission factor, Darkened
 7.0 %
@Thickness 2.00 mm
Solar UV-A transmission factor, Faded
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
t(max), Faded
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
t(max), Darkened
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
t(avg), Faded
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
t(avg), Darkened
 2.0 %
@Wavelength 315 - 350 nm,
Thickness 2.00 mm
t(max), Darkened
 3.0 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
t(moy), Darkened
 5.0 %
@Wavelength 315 - 350 nm,
Thickness 2.00 mm
t(max), Faded
 10 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
t(moy), Faded
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
96% Silica Consolidated Reconstructed Glass
Borosilicate Glass
Corning FUSIBLE PHOTOGRAY THIN&DARK ™ Wide range photochromic glass for thin lenses
Corning FUMO 15 Tinted Optical Glass
Corning 1.8 / 35 BLANC High Index glass

CCORN929 / 233340

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.