Product Description: FRblend® PBT-1306 is an unfilled, halogen-free, flame retardant polybutylene -terephathalate compound. The flame retardant system is based on non-chlorinated and non-brominated. Features: - Flame retardant
- Chlorine free
- Bromine free
Uses:- Switches
- Connectors
- Electrical/electronic applications