KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from the fine powder form. KetaSpire® PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, ease of melt processing, high purity, and excellent chemical resistance to organics, acids, and bases. These properties make it well-suited for applications in healthcare, transportation, electronics, chemical processing, and other industrial uses. The resin is also available as KetaSpire KT-880 NT in a natural-color pellet form for injection molding. Applications: Aircraft Applications; Connectors; Dental Applications; Electrical/Electronic Applications; Film; Hospital Goods; Industrial Applications; Medical Devices; Medical/Healthcare Applications; Oil/Gas Applications; Pump Parts; Seals; Surgical Instruments Features: Autoclave Sterilizable; Biocompatible; Chemical Resistant; Ductile; E-beam Sterilizable; Ethylene Oxide Sterilizable; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; Good Impact Resistance; Good Sterilizability; Heat Sterilizable; High Flow; High Heat Resistance; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam Sterilizable The particle size distribution is such that no particle is larger than 149 microns, and less than 2% of the weight of the material is larger than 106 microns. Information provided by Solvay Specialty Polymers. |