MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Stat-Rite® S-1110 Polyethylene
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Product Description: S-1110 Polymers is an Inherently Dissipative Polymer (IDP) specially developed using Lubrizol’s patented Stat-Rite® IDP technology to impart permanent static dissipative property to polyethylene resins. Blend of Stat-Rtie® S-1110 with polyethylene can be directly injection molded or extruded into the desired products. Typical loading of 10-25% shall impart surface resistivities of 10E9 – 10E11 ohm/square to the final products. Features: Permanently static dissipative; Humidity independent. Applications: Cleanroom accessories; Electronic equipment parts and housing
Availability: Asia Pacific, Europe, Latin America, North America
Features: Antistatic; Humidity Independent; Rapid Static Decay
Uses: Electrical Housing; Electrical Parts; Electrical/Electronic Applications; Housings; Masterbatch
Appearance: Yellow
Forms: Pellets
Processing Method: Extrusion; Injection Molding

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
Melt Flow 65 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 800 psiASTM D638
Elongation at Break >= 500 %ASTM D638
Flexural Modulus 20000 psiASTM D790
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 5.00e+6 ohm12% RH; ESD S11.11
Surface Resistivity per Square 5.00e+7 ohm12% RH; ESD S11.11
Static Decay 0.10 sec1000 V to 100 V, CPM, 50% RH
 0.10 sec1000 V to 10 V, CPM, 50% RH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBR6020 / 268322

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.