MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lord Adhesives Chemlok® 206 Blue Primer and/or Adhesive
Categories: Polymer

Material Notes: LORD Chemlok® 206 Blue primer is designed for use under Chemlok covercoat adhesives to bond a wide variety of vulcanized and unvulcanized rubber compounds to metals and other rigid substrates. It is composed of a mixture of polymers, organic compounds and mineral fillers dissolved or dispersed in an organic solvent system. Chemlok 206 Blue primer requires no additional reduction.

Features: can be used as a primer under a wide variety of Chemlok covercoat adhesives such as the Chemlok 220 series, Chemlok 230 series, Chemlok 250 series or Chemlok 6000 series adhesives. applies easily by brush, dip, spray or roll coat methods; suitable for existing production lines; ready to use directly out of container without dilution, reducing cost and simplifying application process. provides rubber tearing bonds and excellent environmental resistance when used in combination with Chemlok covercoat adhesives.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.70 - 8.10 lb/gal
Solids Content 22 - 26 %by weight
Brookfield Viscosity 25 - 250 cP
@Temperature 25.0 °C
Brookfield LVT, Spindle 2, 30 rpm
 
Thermal PropertiesOriginal ValueComments
Flash Point 19.0 °CSeta
 
Processing PropertiesOriginal ValueComments
Shelf Life 3.00 Month
@Temperature 21.0 - 27.0 °C
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceBlue liquid
SolventsMethyl Isobutyl Ketone (MIBK), Methyl Ethyl Ketone (MEK), Xylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9026 / 232415

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.