MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Asahi Kasei Tenac®-C TFC64 Copolymer Acetal Resin  (Unverified Data**)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Electro Conductive grade

Information provided by Asahi Kasei Corporation.

Key Words: Tenac-C
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccISO 1183
Linear Mold Shrinkage 0.013 - 0.016 cm/cmAsahi Kasei Method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 35.0 MPaISO 527 - 1 & - 2
Elongation at Break 2.0 %ISO 527 - 1 & - 2
Tensile Modulus 2.20 GPaISO 527 - 1 & - 2
Charpy Impact, Notched 0.300 J/cm²ISO 179 / 1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.0 - 100 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 146 °CISO 75 -1 & -2 flat
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °CISO 75 -1 & -2 flat
Flammability, UL94 HB

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kolon KOCETAL® CB301 Conductive Grade Acetal Resin
Polyplastics Duracon® SW-01 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding
Asahi Kasei TENAC™-C TFC64 Copolymer Acetal (POM), Electrically Conductive
Asahi Kasei Tenac®-C EF450 Copolymer Polyacetal Resin
Asahi Kasei Lynex-T TFC64N Acetal Copolymer, Conductive Grade

PLA9AS047 / 49748

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.