MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Marco Polo MARPOL P1868 Polyolefin Elastomer
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: MARPOL P1868 is an ethylene octene copolymer produced by solution polymerization using metallocene catalyst. This product is available as free flowing pellets. It is designed as a low density and high performance copolymer modifier to provide superior impact properties and flow characteristics.

Applications: Impact modification in thermoplastic olefin compounds, injection molded industrial and consumer durable goods, wire and cable and footwear.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.868 g/ccASTM D792
Mooney Viscosity 22
@Temperature 121 °C
[MU], ML 1+4; ASTM D 1646
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 71ASTM D2240
Hardness, Shore D 21ASTM D2240
Tensile Strength at Break 9.30 MPaASTM D 638
Elongation at Break 850 %ASTM D 638
Tensile Modulus 2.90 MPaASTM D 638
Flexural Modulus, 1% Secant 13.2 MPaASTM D790A
Tear Strength 39.2 kN/mASTM D624
 
Thermal PropertiesOriginal ValueComments
Melting Point 62.0 °CPeak
Glass Transition Temp, Tg -52.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMARCO001 / 283598

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.