MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Toray AMILAN™ CM3304-V0 Nylon 66, Unreinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Nylon 66/Flame Retardant, unreinforced, halogen, PA66-FR.

General Amilan™ Notes: AMILAN™ nylon (polyamide) is a thermoplastic engineering plastic containing an amide group (-CONH-) and it exhibits excellent strength, toughness, heat resistance, and anti-friction wear resistance. A variety of grades designed for various customer needs and applications are available.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³Dry; ISO 1183
Water Absorption 8.0 %8.0 %In 23°C water, polymer initally dry; ISO 62
 1.2 %
@Time 86400 sec
1.2 %
@Time 24.0 hour
In 23°C water, polymer initally dry; ISO 62
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/in80x80x1mmt. 1.8% Moisture Content; Toray Method
 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/in80x80x1mmt. Dry; Toray Method
 0.010 - 0.014 cm/cm0.010 - 0.014 in/in80x80x3mmt. 1.8% Moisture Content; Toray Method
 0.010 - 0.014 cm/cm0.010 - 0.014 in/in80x80x3mmt. Dry; Toray Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120
@Temperature 23.0 °C
120
@Temperature 73.4 °F
Dry; ISO 2039-2
Tensile Strength  55.0 MPa
@Temperature 23.0 °C
7980 psi
@Temperature 73.4 °F
1.8% Moisture Content; ISO 527-1,2
 75.0 MPa
@Temperature 23.0 °C
10900 psi
@Temperature 73.4 °F
Dry; ISO 527-1,2
Elongation at Break  3.5 %
@Temperature 23.0 °C
3.5 %
@Temperature 73.4 °F
Dry; ISO 527-1,2
 6.0 %
@Temperature 23.0 °C
6.0 %
@Temperature 73.4 °F
1.8% Moisture Content; ISO 527-1,2
Flexural Strength  60.0 MPa
@Temperature 23.0 °C
8700 psi
@Temperature 73.4 °F
1.8% Moisture Content; ISO 178
 110 MPa
@Temperature 23.0 °C
16000 psi
@Temperature 73.4 °F
Dry; ISO 178
Flexural Modulus  1.30 GPa
@Temperature 23.0 °C
189 ksi
@Temperature 73.4 °F
1.8% Moisture Content; ISO 178
 2.90 GPa
@Temperature 23.0 °C
421 ksi
@Temperature 73.4 °F
Dry; ISO 178
Charpy Impact, Notched  0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
V-Notched. Dry; ISO 179
 0.950 J/cm²
@Temperature 23.0 °C
4.52 ft-lb/in²
@Temperature 73.4 °F
V-Notched. 1.8% Moisture Content; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmDry; IEC 60093
Dielectric Strength 25.0 kV/mm635 kV/inDry; IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C55.6 µin/in-°FDry; ISO 11359-2
Melting Point 244 °C471 °FDry; DSC Method
Flammability, UL94  V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
1.8% Moisture Content
 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
Dry

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY9126 / 248816

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.